新疆产棉区高强棉纤维形成的纤维素累积特征及适宜温度
|
田景山,张煦怡,虎晓兵,随龙龙,张鹏鹏,王文敏,勾玲,张旺锋
|
Cellulose Deposition Characteristics of High Strength Cotton Fiber and Optimal Temperature Requirements in Xinjiang Region
|
TIAN JingShan,ZHANG XuYi,HU XiaoBing,SUI LongLong,ZHANG PengPeng,WANG WenMin,GOU Ling,ZHANG WangFeng
|
|
表4 棉纤维发育不同阶段的温度因子与纤维素累积特征的相关分析
|
Table 4 Correlation analysis of factors affecting cellulose deposition at different fiber development stages of cotton fiber (period I and II)
|
|
纤维素累积阶段 Period of cotton fiber development | 纤维素特征值 Cellulose deposition parameters | 最低温度 Daily minimum temperature | 最高温度 Daily maximum temperature | 平均温度 Average temperature | ≥15℃有效积温 Growing degree days | 日温差 Diurnal temperature range | I 段区 Period I | t1 | -0.1511 | 0.0075 | -0.0078 | 0.8236** | 0.1807 | (0—t1) | V1 | 0.2041 | 0.1679 | 0.1700 | -0.6589** | -0.0453 | | Wm | 0.0994 | 0.2906 | 0.2730 | -0.0926 | 0.2228 | | Str | -0.1299 | -0.1067 | -0.1332 | -0.3696* | 0.0295 | II 段区 Period II | t2 | -0.6825** | -0.4674** | -0.5690** | 0.1098 | 0.4931** | (t1—t2) | T | -0.3723* | -0.2861 | -0.2945 | 0.6738** | 0.2178 | | Vt | 0.6543** | 0.6358** | 0.6341** | -0.2759 | -0.1300 | | Wm | 0.4187* | 0.6011** | 0.5526** | 0.5674** | 0.2887 | | V1 | 0.4703** | 0.3247 | 0.4409** | 0.7481** | -0.3277 | | Str | 0.1215 | 0.1480 | 0.1349 | 0.3636* | 0.0399 |
|
|
|